Hi all,
Was wondering what is the ideal printing temperature you've been using for PET-CF for strongest layer adhesion?
Regarding Siraya Tech PET-CF, I've been successfully printing it through a hardened steel 0.4mm nozzle at 275 Deg C with excellent cosmetic print quality (Bambu P1S). But, I don't know if the layer adhesion is adequate for the SL-15 and SL-9.
Finally, is nozzle size for PET-CF primarily addressing clogging or are there other benefits such as improved layer adhesion when using a 0.6mm nozzle vs a 0.4mm nozzle.
Your insight is appreciated.
Thanks